Aluminum - Thermophysical Properties

Sponsored Links
Aluminum - Thermophysical Properties
T
(K)
ρ
(kg/m³)
c
(kJ/kg K)
k
(W/m K)
150 2726 0.683 250
200 2719 0.797 237
250 2710 0.859 235
300 2701 0.902 237
400 2681 0.949 240
600 2639 1.042 231
Sponsored Links

Related Topics

Material Properties

Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Aluminum - Melting Points of Binary Eutectic Alloys

Al - Aluminum - binary eutectic alloys and their melting points.

Aluminum - Radiation Heat Emissivity

Radiation heat emissivity of unoxidized, oxidized and polished aluminum.

Aluminum Alloys - Mechanical Properties

Mechanical properties of aluminum alloys - tensile strength, yield strength and more.

Aluminum Alloys - Mechanical Properties

Mechanical properties of some common aluminum alloys.

Aluminum Channels

Dimensions and static parameters of aluminum channels.

Aluminum Conductor Characteristics

Characteristics of all-aluminum conductors (AAC).

Metals - Specific Heats

Specific heat of commonly used metals like aluminum, iron, mercury and many more - imperial and SI units.

Metals - Temperature Expansion Coefficients

Thermal expansion coefficients metals.

Metals and Alloys - Densities

Densities of some common metals, metallic elements and alloys - aluminum, bronze, copper, iron and more.

Thermal Conductivity of Metals and Alloys: Data Table & Reference Guide

Thermal conductivities of common metals, metallic elements and alloys.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.