Metals - Boiling Temperatures
Boiling temperatures for some metals are indicated below:
Metal | Boiling Temperature | |
---|---|---|
(oF) | (oC) | |
Aluminum | 4478 | 2470 |
Antimony | 2625 | 1440 |
Beryllium | 4487 | 2475 |
Cadmium | 1413 | 767 |
Chromium | 4838 | 2670 |
Cobalt | 5297 | 2925 |
Copper | 4667 | 2575 |
Gold | 5072 | 2800 |
Iron | 5198 | 2870 |
Lead | 3182 | 1750 |
Magnesium | 1994 | 1090 |
Manganese | 3740 | 2060 |
Mercury | 675 | 357 |
Molybdenum | 8403 | 4651 |
Nickel | 5072 | 2800 |
Niobium | 8564 | 4740 |
Platinum | 4098 | 3825 |
Plutonium | 5846 | 3230 |
Potassium | 1400 | 760 |
Rhodium | 6692 | 3700 |
Selenium | 1292 | 700 |
Silicon | 5936 | 3280 |
Silver | 4013 | 2212 |
Sodium | 1623 | 884 |
Tantalum | 9689 | 5365 |
Thorium | 8672 | 4800 |
Tin | 4712 | 2600 |
Titanium | 5954 | 3290 |
Tungsten | 10022 | 5550 |
Uranium | 7484 | 4140 |
Zinc | 1670 | 910 |
Related Topics
• Boiling Points of Fluids
Boiling points of elements, products and chemical species at varying conditions.
• Material Properties
Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.
Related Documents
Hydrocarbons, Alcohols and Acids - Boiling points
Boiling temperatures (°C and °F) with varying carbon numbers up to C33.
Magnesium Binary Eutectic Alloys - Melting Points
Mg - Magnesium - binary eutectic alloys and melting points.
Metals - Latent Heat of Melting
Metals and their latent heat of fusion.
Metals - Specific Heats
Specific heat of commonly used metals like aluminum, iron, mercury and many more - imperial and SI units.
Metals - Temperature Expansion Coefficients
Thermal expansion coefficients metals.
Metals and Alloys - Melting Temperatures
The melting temperatures for some common metals and alloys.
Solids and Metals - Specific Gravities
Specific gravity for common solids and metals like aluminum, asbestos, brass, calcium and many others.
Thermal Conductivity of Metals and Alloys: Data Table & Reference Guide
Thermal conductivities of common metals, metallic elements and alloys.