Trees commonly used in towns and urban areas:
Tree Specie | Normal Height (m) | |
---|---|---|
after 25 years | as mature | |
Acacia | 14 | 21 |
Ailanthus | 18 | 21 |
Almond | 7 | 8 |
Birch | 10 | 18 |
Catalpa | 10 | 12 |
Cherry, gean | 12 | 15 |
Cherry, bird | 7 | 14 |
Chestnut | 7 | 12 |
Crab apple | 6 | 12 |
Hawthorn | 6 | 8 |
Lime | 10 | 18 |
Maidenhair | 7 | 30 |
Maple, field | 7 | 10 |
Maple, silver | 15 | 25 |
Mountain ash | 7 | 8 |
Oak, evergreen | 7 | 28 |
Oak, scarlet | 15 | 18 |
Plane | 12 | 28 |
Sycamore | 12 | 25 |
Tulip tree | 12 | 30 |
Whitebeam | 7 | 12 |
Related Topics
• Environment
Climate, meteorology, solar, wind, emissions and environmental related engineering resources.
• Miscellaneous
Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.
Related Documents
Density of Wood Species: Data & Material Guide
Densities of various wood species - apple, ash, cedar, elm and more.
Fire Wood - the Cord
The cord unit for purchasing fuel wood.
Structural Lumber - Properties
Properties of structural lumber.
Tree Species - Water Demand
Trees species and relative water demand.
Wood - Combustion Heat Values
Combustion of wood and firewood heat values for species like Pine, Elm, Hickory and more.
Wood - Density vs. Moisture Content
The density of wood versus moisture content.
Wood and Bio Mass - Combustion Heat
Combustion heat values for wet and dry wood - Btu/pounds, kJ/kg and kcal/kg.
Wood Beams - Strength of Material
Bending and compression strength of wood species used in beams.
Wood Columns - Safe Loads
Safe loads for wood columns.
Wood Hardness
Soft and hardwood - the Janka Hardness scale.
Wood Species - Moisture Content and Weight
Weight of green and air-dried fire wood.