Surface | Absorptivity |
---|---|
Aluminum, anodized | 0.14 |
Aluminum, dull/rough polished | 0.4 - 0.65 |
Aluminum. polished | 0.1 - 0.40 |
Asbestos Cement, old | 0.83 |
Black matte | 0.95 |
Brick, red | 0.65 |
Chromium plate | 0.20 |
Concrete | 0.6 |
Iron, galvanized old | 0.89 - 0.92 |
Grey paint | 0.95 |
Light green paint | 0.95 |
Limestone | 0.33 - 0.53 |
Red clay brick | 0.94 |
Snow, ice granules | 0.33 |
Steel, galvanized (zink oxide) | 0.65 |
Steel, galvanized weathered | 0.8 |
White paint | 0.25 - 0.4 |
Related Topics
• Thermodynamics
Work, heat and energy systems.
Related Documents
Absorbed Solar Radiation
Solar radiation absorbed by various materials.
Aluminum - Radiation Heat Emissivity
Radiation heat emissivity of unoxidized, oxidized and polished aluminum.
Building Materials - Radiation Constants
The radiation constant is the product between the Stefan-Boltzmann constant and the emissivity constant for a material.
Emissivity Coefficients of Common Materials: Data & Reference Guide
The radiation heat transfer emissivity coefficients for some common materials like aluminum, brass, glass and many more.
Radiation - Surface Emissivity Coefficients
Radiation emissivity of common materials like water, ice, snow, grass and more.
Radiation Heat Transfer
Heat transfer due to emission of electromagnetic waves is known as thermal radiation.
Solar Radiation - Daily Surface Energy
Daily surface energy from solar radiation.
Solar Radiation through Windows
Heat from sun transmitted through windows.