Foods - Thermal Conductivities

Sponsored Links

Conduction as heat transfer takes place if there is a temperature gradient in a solid or stationary fluid medium.

Thermal conductivity of some selected food products:

Foods - Water Content and Thermal Conductivities
FoodWater Content
(%)
Temperature
(oC)
Thermal Conductivity
(W/(m K))
Apple, whole 85 2 - 35 0.39
Apple, juice 88 20 0.56
Beef, freeze dried, 1 bar 0 0.07
Beef, freeze dried, 10-6 bar 0 0.04
Beef, lean, perpendicular to fibers 79 7 0.48
Beef, lean, parallel to fibers 79 7 0.43
Butter 15 45 0.2
Cod 83 3 0.54
Egg, white 35 0.58
Egg, yolk 35 0.34
Fish, loin 0 - 10 0.58
Grapefruit, whole 30 0.45
Honey 13 2 0.50
Milk 37 0.53
Milk, condensed 90 24 0.57
Milk, skimmed 2 0.54
Olive oil 15 0.19
Pork, perpendicular to fibers 75 5 0.49
Pork, parallel to fibers 75 5 0.44
Pork, fat 25 0.15
Potato, raw flesh 82 1 - 35 0.55
Poultry, broiler muscle 70 4 - 25 0.41
Salmon 75 4 0.50
Salt 90 0.25
Strawberry 15 - 25 0.68
Sugars 30 - 60 0.09 - 0.22
Turkey, breast prependicular to fibers 75 3 0.50
Turkey, breast parallel to fibers 75 3 0.52
Oil, vegetable and animal 4 - 180 0.17
Wheat flour 9 43 0.45
Whey 80 0.64
Sponsored Links

Related Topics

Material Properties

Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Conductive Heat Transfer

Conductive heat transfer takes place in a solid if there is a temperature gradient.

Drying Temperatures and Times for Various Products

Drying temperature and time for products like food, coffee, fruits, lumber and more.

Food and Foodstuff - pH Values

pH in common food products - like apples, butter, wines and more.

Food and Foodstuff - Specific Heat

Specific heat of common food and foodstuff like apples, bass, beef, pork and many more.

Food Products - Bulk Densities

Bulk densities of some common food products like grain, corn, barley, sugar and more.

Food Products - Osmotic Pressures

Osmotic pressure in food products.

Food Products - Viscosities

Absolute (dynamic) viscosity for common food products.

Foodstuff - Thermal Diffusivity

Thermal diffusivity of some selected food products.

Frozen Food - Storage Life

Practical storage life for common frozen food products.

Fruits and Vegetables - Optimal Storage Conditions

Optimal temperature and humidity conditions for common fruits and vegetables.

Microwave Heating

Heating with microwaves.

Pasteurization - Temperatures and Time

Pasteurization methods, time and temperatures.

Thermal Conductivity of Common Materials - Solids, Liquids and Gases

Thermal conductivity of various common materials, including metals, gases, and building materials. Essential data for engineers, architects, and designers working with heat transfer and insulation.

Thermal Conductivity of Metals and Alloys: Data Table & Reference Guide

Thermal conductivities of common metals, metallic elements and alloys.

Water Content in Food and other Products

Water content before and after drying - in food and other products cork, grain, soap, peat, wood and more.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.