W-beams - wide flange beams - are stout, sturdy beams with wide flanges positioned perpendicularly to the web of the material giving them their characteristic shape and distinguishing them from I-beams.

Properties in imperial units of American Wide Flange Beams according ASTM A6 are indicated below.

For full table with Depth, Width, Web and Flange Thickness and Section Area - rotate the screen!

W-Beams - American Wide Flange Beams - Static Parameters
Designation
Imperial
(in x lb/ft)

Depth
h
(in)
Width
w
(in)
Web Thickness
tw
(in)
Flange Thickness
tf
(in)
Sectional Area
(in2)
Weight
(lbf/ft)
Static Parameters
Moment of InertiaElastic Section Modulus
Ix
(in4)
Iy
(in4)
Sx
(in3)
Sy
(in3)
W 27 x 178 27.8 14.09 0.725 1.190 52.3 178 6990 555 502 78.8
W 27 x 161 27.6 14.02 0.660 1.080 47.4 161 6280 497 455 70.9
W 27 x 146 27.4 14 0.605 0.975 42.9 146 5630 443 411 63.5
W 27 x 114 27.3 10.07 0.570 0.930 33.5 114 4090 159 299 31.5
W 27×102 27.1 10.02 0.515 0.830 30.0 102 3620 139 267 27.8
W 27 x 94 26.9 10 0.490 0.745 27.7 94 3270 124 243 24.8
W 27 x 84 26.7 9.96 0.460 0.640 24.8 84 2850 106 213 21.2
                   
W 24 x 162 25 13 0.705 1.220 47.7 162 5170 443 414 68.4
W 24 x 146 24.7 12.9 0.650 1.090 43.0 146 4580 391 371 60.5
W 24 x 131 24.5 12.9 0.605 0.960 38.5 131 4020 340 329 53.0
W 24 x 117 24.3 12.8 0.55 0.850 34.4 117 3540 297 291 46.5
W 24×104 24.1 12.75 0.500 0.750 30.6 104 3100 259 258 40.7
W 24 x 94 24.1 9.07 0.515 0.875 27.7 94 2700 109 222 24.0
W 24 x 84 24.1 9.02 0.470 0.770 24.7 84 2370 94.4 196 20.9
W 24 x 76 23.9 9 0.440 0.680 22.4 76 2100 82.5 176 18.4
W 24 x 68 23.7 8.97 0.415 0.585 20.1 68 1830 70.4 154 15.7
W 24 x 62 23.7 7.04 0.430 0.590 18.2 62 1550 34.5 131 9.8
W 24 x 55 23.6 7.01 0.395 0.505 16.2 55 1350 29.1 114 8.3
                   
W 21 x 147 22.1 12.51 0.720 1.150 43.2 147 3630 376 329 60.1
W 21 x 132 21.8 12.44 0.650 1.035 38.8 132 3220 333 295 53.5
W 21 x 122 21.7 12.39 0.600 0.960 35.9 122 2960 305 273 49.2
W 21 x 111 21.5 12.34 0.550 0.875 32.7 111 2670 274 249 44.5
W 21×101 21.4 12.29 0.500 0.800 29.8 101 2420 248 227 40.3
W 21 x 93 21.6 8.42 0.580 0.930 27.3 93 2070 92.9 192 22.1
W 21 x 83 21.4 8.36 0.515 0.835 24.3 83 1830 81.4 171 19.5
W 21 x 73 21.2 8.3 0.455 0.740 21.5 73 1600 70.6 151 17.0
W 21 x 68 21.1 8.27 0.430 0.685 20.0 68 1480 64.7 140 15.7
W 21 x 62 21 8.24 0.400 0.615 18.3 62 1330 57.5 127 13.9
W 21 x 57 21.1 6.56 0.405 0.650 16.7 57 1170 30.6 111 9.4
W 21 x 50 20.8 6.53 0.380 0.535 14.7 50 984 24.9 94.5 7.6
W 21 x 44 20.7 6.5 0.350 0.450 13.0 44 843 20.7 81.6 6.4
                   
W 18 x 119 19 11.27 0.655 1.060 35.1 119 2190 253 231 44.9
W 18×106 18.7 11.2 0.590 0.940 31.1 106 1910 220 204 39.4
W 18 x 97 18.6 11.15 0.535 0.870 28.5 97 1750 201 188 36.1
W 18 x 86 18.4 11.09 0.480 0.770 25.3 86 1530 175 166 31.6
W 18 x 76 18.2 11.04 0.425 0.680 22.3 76 1330 152 146 27.6
W 18 x 71 18.5 7.64 0.495 0.810 20.8 71 1170 60.3 127 15.8
W 18 x 65 18.4 7.59 0.450 0.750 19.1 65 1070 54.8 117 14.4
W 18 x 60 18.2 7.56 0.415 0.695 17.6 60 984 50.1 108 13.3
W 18 x 55 18.1 7.53 0.390 0.630 16.2 55 890 44.9 98.3 11.9
W 18 x 50 18 7.5 0.355 0.570 14.7 50 800 40.1 88.9 10.7
W 18 x 46 18.1 6.06 0.360 0.605 13.5 46 712 22.5 78.8 7.4
W 18 x 40 17.9 6.02 0.315 0.525 11.8 40 612 19.1 68.4 6.4
W 18 x 35 17.7 6 0.300 0.425 10.3 35 510 15.3 57.6 5.1
                   
W 16×100 16.97 10.425 0.585 0.985 29.4 100 1490 186 175 35.7
W 16 x 89 16.75 10.365 0.525 0.875 26.2 89 1300 163 155 31.4
W 16 x 77 16.52 10.295 0.455 0.760 22.6 77 1100 138 134 26.9
W 16 x 67 16.33 10.235 0.395 0.665 19.7 67 954 119 117 23.2
W 16 x 57 16.43 7.120 0.430 0.715 16.8 57 758 43.1 92.2 12.1
W 16 x 50 16.26 7.070 0.380 0.630 14.7 50 659 37.2 81 10.5
W 16 x 45 16.13 7.035 0.345 0.565 13.3 45 586 32.8 72.7 9.3
W 16 x 40 16.01 6.995 0.305 0.505 11.8 40 518 28.9 64.7 8.3
W 16 x 36 15.86 6.985 0.295 0.430 10.6 36 448 24.5 56.5 7
W 16 x 31 15.88 5.525 0.275 0.440 9.12 31 375 12.4 47.2 4.5
W 16 x 26 15.69 5.5 0.250 0.345 7.68 26 301 9.6 38.4 3.5
                   
W 14 x 132 14.66 14.725 0.645 1.030 38.8 132 1530 548 209 74.5
W 14 x 120 14.48 14.670 0.590 0.940 35.3 120 1380 495 190 67.5
W 14×109 14.32 14.605 0.525 0.860 32 109 1240 447 173 61.2
W 14 x 99 14.16 14.565 0.485 0.780 29.1 99 1110 402 157 55.2
W 14 x 90 14.02 14.520 0.440 0.710 26.5 90 999 362 143 49.9
W 14 x 82 14.31 10.130 0.510 0.855 24.1 82 882 148 123 29.3
W 14 x 74 14.17 10.070 0.450 0.785 21.8 74 796 134 112 26.6
W 14 x 68 14.04 10.035 0.415 0.720 20.0 68 723 121 103 24.2
W 14 x 61 13.89 9.995 0.375 0.645 17.9 61 640 107 92.2 21.5
W 14 x 53 13.92 8.060 0.370 0.660 15.6 53 541 57.7 77.8 14.3
W 14 x 48 13.79 8.030 0.340 0.595 14.1 48 485 51.4 70.3 12.8
W 14 x 43 13.66 7.995 0.305 0.530 12.6 43 428 45.2 62.7 11.3
W 14 x 38 14.10 6.770 0.310 0.515 11.2 38 385 26.7 54.6 7.9
W 14 x 34 13.98 6.745 0.285 0.455 10.0 34 340 23.3 48.6 6.9
W 14 x 30 13.84 6.730 0.270 0.385 8.85 30 291 19.6 42.0 5.8
W 14 x 26 13.91 5.025 0.255 0.420 7.69 26 245 8.9 35.3 3.5
W 14 x 22 13.74 5 0.230 0.335 6.49 22 199 7 29.0 2.8
                   
W 12 x 136 13.41 12.4 0.79 1.250 39.9 136 1240 398 186 64.2
W 12 x 120 13.12 12.32 0.71 1.105 35.3 120 1070 345 163 56.0
W 12×106 12.89 12.22 0.61 0.990 31.2 106 933 301 145 49.3
W 12 x 96 12.71 12.16 0.55 0.900 28.2 96 833 270 131 44.4
W 12 x 87 12.53 12.125 0.515 0.810 25.6 87 740 241 118 39.7
W 12 x 79 12.38 12.08 0.47 0.735 23.2 79 662 216 107 35.8
W 12 x 72 12.25 12.04 0.43 0.670 21.1 72 597 195 97.4 32.4
W 12 x 65 12.12 12 0.39 0.605 19.1 65 533 174 87.9 29.1
W 12 x 58 12.19 10.01 0.36 0.640 17.0 58 475 107 78 21.4
W 12 x 53 12.06 9.995 0.345 0.575 15.6 53 425 95.8 70.6 19.2
W 12 x 50 12.19 8.08 0.37 0.640 14.7 50 394 56.3 64.7 13.9
W 12 x 45 12.06 8.045 0.335 0.575 13.2 45 350 50.0 58.1 12.4
W 12 x 40 11.94 8.005 0.295 0.515 11.8 40 310 44.1 51.9 11.0
W 12 x 35 12.50 6.56 0.3 0.520 10.3 35 285 24.5 45.6 7.5
W 12 x 30 12.34 6.52 0.26 0.440 8.8 30 238 20.3 38.6 6.2
W 12 x 26 12.22 6.490 0.23 0.380 7.7 26 204 17.3 33.4 5.3
W 12 x 22 12.31 4.03 0.26 0.425 6.5 22 156 4.7 25.4 2.3
W 12 x 19 12.16 4.005 0.235 0.350 5.6 19 130 3.8 21.3 1.9
W 12 x 16 11.99 3.990 0.22 0.265 4.7 16 103 2.8 17.1 1.4
W 12 x 14 11.91 3.970 0.2 0.225 4.2 14 88.6 2.4 14.9 1.2
                   
W 10 x 112 11.36 10.415 0.755 1.250 32.9 112 716 236 126 45.3
W 10×100 11.1 10.340 0.680 1.1120 29.4 100 623 207 112 40.0
W 10 x 88 10.84 10.265 0.605 0.990 25.9 88 534 179 98.5 34.8
W 10 x 77 10.60 10.190 0.530 0.870 22.6 77 455 154 85.9 30.1
W 10 x 68 10.40 10.130 0.470 0.770 20.0 68 394 134 75.7 26.4
W 10 x 60 10.22 10.080 0.420 0.680 17.6 60 341 116 66.7 23.0
W 10 x 54 10.09 10.030 0.370 0.615 15.8 54 303 103 60.0 20.6
W 10 x 49 9.98 10 0.340 0.560 14.4 49 272 93.4 54.6 18.7
W 10 x 45 10.10 8.020 0.350 0.620 13.3 45 248 53.4 49.1 13.3
W 10 x 39 9.92 7.985 0.315 0.530 11.5 39 209 45.0 42.1 11.3
W 10 x 33 9.73 7.960 0.290 0.435 9.71 33 170 36.6 35.0 9.2
W 10 x 30 10.47 5.81 0.3 0.510 8.84 30 170 16.7 32.4 5.8
W 10 x 26 10.33 5.770 0.26 0.440 7.6 26 144 14.1 27.9 4.9
W 10 x 22 10.17 5.750 0.240 0.360 6.5 22 118 11.4 23.2 4
W 10 x 19 10.24 4.020 0.250 0.395 5.6 19 96.3 4.3 18.8 2.1
W 10 x 17 10.11 4.010 0.240 0.330 5 17 81.9 3.6 16.2 1.8
W 10 x 15 9.99 4 0.230 0.270 4.4 15 68.9 2.9 13.8 1.5
W 10 x 12 9.87 3.960 0.190 0.210 3.5 12 53.8 2.2 10.9 1.1
                   
W 8 x 67 9.00 8.280 0.570 0.935 19.7 67 272 88.6 60.4 21.4
W 8 x 58 8.75 8.220 0.510 0.810 17.1 58 228 75.1 52.0 18.3
W 8 x 48 8.5 8.110 0.400 0.685 14.1 48 184 60.9 43.3 15.0
W 8 x 40 8.25 8.070 0.360 0.560 11.7 40 146 49.1 35.5 12.2
W 8 x 35 8.12 8.020 0.310 0.495 10.3 35 127 42.6 31.2 10.6
W 8 x 31 8.00 7.995 0.285 0.435 9.1 31 110 37.1 27.5 9.3
W 8 x 28 8.06 6.535 0.285 0.465 8.3 28 98.0 21.7 24.3 6.6
W 8 x 24 7.93 6.495 0.245 0.400 7.1 24 82.8 18.3 20.9 5.6
W 8 x 21 8.28 5.270 0.250 0.400 6.2 21 75.3 9.8 18.2 3.7
W 8 x 18 8.14 5.250 0.230 0.330 5.3 18 61.9 8 15.2 3
W 8 x 15 8.11 4.015 0.245 0.315 4.4 15 48.0 3.4 11.8 1.7
W 8 x 13 7.99 4 0.230 0.255 3.8 13 39.6 2.7 9.9 1.4
W 8×10 7.89 3.940 0.170 0.205 2.9 10 30.8 2.1 7.8 1.1
                   
W 6 x 25 6.38 6.080 0.320 0.455 7.3 25 53.4 17.1 16.7 5.6
W 6 x 20 6.20 6.020 0.260 0.365 5.9 20 41.4 13.3 13.4 4.4
W 6 x 16 6.28 4.030 0.260 0.405 4.7 16 32.1 4.4 10.2 2.2
W 6 x 15 5.99 5.990 0.230 0.260 4.4 15 29.1 9.3 9.7 3.1
W 6 x 12 6.03 4 0.230 0.280 3.6 12 22.1 3 7.3 1.5
W 6 x 9 5.90 3.940 0.170 0.215 2.7 9 16.4 2.2 5.6 1.1
                   
W 5 x 19 5.15 5.030 0.270 0.430 5.5 19 26.2 9.1 10.2 3.6
W 5 x 16 5.01 5 0.240 0.360 4.7 16 21.3 7.5 8.5 3
                   
W 4 x 13 4.16 4.060 0.280 0.345 3.8 13 11.3 3.9 5.5 1.9
  • 1 cm4 = 10-8 m = 104 mm
  • 1 in4 = 4.16×105 mm4 = 41.6 cm4
  • 1 cm3 = 10-6 m = 103 mm
.

Calculate Loads

The standard method for specifying the dimensions of a American Wide Flange Beam is for example W 6 x 25, which is 6 inches deep with a weight of 25 lb/ft.

I-shaped cross-section beams:

  • Britain : Universal Beams (UB) and Universal Columns (UC)
  • Europe : IPE. HE. HL. HD and other sections
  • US : Wide Flange (WF) and H sections

Insert W beams to your 3D Sketchup model with the Engineering ToolBox Sketchup Extension

Sponsored Links

Related Topics

Beams and Columns

Deflection and stress in beams and columns, moment of inertia, section modulus and technical information.

Mechanics

The relationships between forces, acceleration, displacement, vectors, motion, momentum, energy of objects and more.

Related Documents

American Standard Beams - S Beam

American Standard Beams ASTM A6 - Imperial units.

American Standard Steel Channels: Weight, Dimensions & Properties

Dimensions and static parameters of American Standard Steel C Channels

American Wide Flange Steel Beams: Dimensions and Properties (ASTM A6 in Metric)

American Wide Flange Beams ASTM A6 in metric units.

Area Moment of Inertia - Typical Cross Sections II

Area Moment of Inertia, Moment of Inertia for an Area or Second Moment of Area for typical cross section profiles.

Area Moment of Inertia with Definitions, Formulas & Calculator

Explore the area moment of inertia (second moment of area) with detailed formulas, calculation tools, and reference tables for common shapes. Essential for structural and mechanical engineering applications.

Beam Loads - Support Force Calculator

Calculate beam load and supporting forces.

Beams - Fixed at One End and Supported at the Other - Continuous and Point Loads

Supporting loads, moments and deflections.

Beams Fixed at Both Ends with Continuous and Point Loads: Load & Deflection Formulas

Stress, deflections and supporting loads.

Beams Supported at Both Ends with Continuous and Point Loads: Stress, Deflection, Formulas and Calculators

Supporting loads, stress and deflections.

British Universal Columns and Beams

Properties of British Universal Steel Columns and Beams.

Drawbridge - Force and Moment vs. Elevation

Calculate the acting forces and moments when elevating drawbridges or beams.

Euler Column Buckling: Formula, Theory & Calculator

Calculate buckling of columns.

HE-A Steel Beams

Properties of HE-A profiled steel beams.

HE-B Steel Beams

Properties of HE-B profiled steel beams.

HE-M Steel Beams

Properties of HE-M profile steel beams.

Normal Flange I-Beams

Properties of normal flange I profile steel beams.

Square Hollow Structural Sections (HSS) – Sizes, Strength & Specifications

Weight, cross sectional area, moments of inertia - Imperial units

Steel Angles - Equal Legs

Dimensions and static parameters of steel angles with equal legs - metric units.

Steel Angles - Unequal Legs

Dimensions and static parameters of steel angles with unequal legs - imperial units.

Steel Angles - Unequal Legs

Dimensions and static parameters of steel angles with unequal legs - metric units.

Steel Flats - Weights

Typically weight of mild steel flats.

Steel Pipe Columns - Allowable Loads

Allowable concentric loads for steel pipe columns.

Steel Plate Weight Guide: Calculator & Data Table

Size & weight of steel plates - Imperial and Metric units.

Trusses

Common types of trusses.

W Steel Beams - Allowable Uniform Loads

Allowable uniform loads.

Weight of Beams - Stress and Strain

Stress and deformation of vertical beams due to own weight.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.