Float Glass - Weight vs. Thickness

Sponsored Links

Weight of float glass:

Float Glass - Weight vs. Thickness
Thickness
(mm)

Weight
(kg/m2)

3 7.5
4 10
5 12.5
6 15
8 20
10 25
12 30
15 37.5
19 47.5
25 62.5
  • Float glass is a sheet of glass made by floating molten glass on a bed of molten metal.
Sponsored Links

Related Topics

Material Properties

Properties of gases, fluids and solids. Densities, specific heats, viscosities and more.

Related Documents

Solar Heat Transmission and Type of Glass

Relative solar heat transmission through different types of glass windows

Windows - Inside Condensation

Water condensation on inside glass windows surfaces vs. outside temperature and inside temperature and humidity.

Sponsored Links

Search Engineering ToolBox

Search is the most efficient way to navigate the Engineering ToolBox!

SketchUp Extension - Online 3D modeling!

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp from the Sketchup Extension Warehouse!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics on the AMP pages. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.