Biomasses - Energy Content when Used as Fuel
Approximately energy content in different biomasses, used as fuels (not prosessed material):
See also Heat of combustion
Bio Fuel | Energy content (MJ/kg) |
---|---|
Alfalfa straw | 18.5 |
Charcoal | 30 |
Coal | 28 |
Coconut husks | 10 |
Coconut shells | 18 |
Coffee husks | 16 |
Commercial wastes | 16 |
Cotton hulls | 19.5 |
Cotton stalks | 17.5 |
Domestic refuse | 9 |
Dung, dried | 16 |
Grass, fresh | 4 |
Groundnut shells | 20 |
Maize cobs | 19 |
Maize stalks | 18 |
Methane from biogas | 55 |
Paper, newspaper | 17 |
Peat | 14.5 |
Petroleum Oil | 42 |
Rice hulls | 15.5 |
Rice straw | 15 |
Soybean stalks | 19 |
Straw, harvested, baled | 15 |
Sorghum bagasse | 19 |
Sugar cane residues | 17 |
Wheat straw | 19 |
Wood, green with 60% moisture | 6 |
Wood, air-dried to 20% moisture | 15 |
Wood, oven-dried to 0% moisture | 18 |
- 1 MJ/kg = 0.28 kWh/kg = 430 Btu/lbm
Wood required to Boil a Litre of Water
The energy to heat one litre of water (1 kg) with specific heat 4.2 kJ/kg oC from 20 oC to boiling 100 oC can be calculated with the heating equation
q = m cp dt (1)
where
q = heat (J, Btu)
m = mass of water (kg, lb)
cp = specific heat of water (J/kg oC, Btu/lb oF)
dt = temperature change (oC,oF)
Inserting the values
q = (1 kg) (4.2 kJ/kg oC ) (1000 J/kJ) (( 100 oC ) - (20 oC ))
= 336000 J
= 336 kJ (kW/s)
= (336 kW/s) / (3600 s/h)
= 0.093 kWh
With energy content of air dryed wood 15 MJ/kg (15000 kJ/kg) and combustion efficiency 0.25 (25%) - the amount of wood to heat the water can be calculated as
mw = q / μ hw (2)
where
mw = mass of wood (kg)
μ = combustion efficiency
hw = energy content wood (kJ/kg)
Inserting the values
mw = (336 kJ) / 0.25 (15000 kJ/kg)
= 0.09 kg
Related Topics
• Combustion
Combustion processes and their efficiency. Boiler house and chimney topics. Properties of fuels like oil, gas, coal and wood and more. Safety valves and tanks.
• Environment
Climate, meteorology, solar, wind, emissions and environmental related engineering resources.
Related Documents
Biogas - Energy Content
Energy content in biogas produced from municipal and industrial waste.
Combustion of Fuels - Carbon Dioxide Emission
Environmental emission of carbon dioxide CO2 when combustion fuels like coal, oil, natural gas, LPG and bio energy.
Copper, Zinc and Tin Alloys
Strength of Copper, Zinc and Tin alloys.
Energy Accumulated in Heated Water - kWh
The amount of thermal energy stored in heated water.
Fire Wood - the Cord
The cord unit for purchasing fuel wood.
Flash Points - Liquids
The flash points for some common liquids and fuels.
Fossil vs. Alternative Fuels - Energy Content
Net (low) and gross (high) energy content in fossil and alternative fuels.
Fuels - Densities and Specific Volumes
Densities and specific volumes fuels like anthracite, butane, gasoil, diesel, coke, oil, wood and more.
Waste Fuel - Heat Values
Fuel from waste products and their heat values.