Dynamic viscosities for motor oils SAE 10 to 50 for temperatures ranging 0-100 oC.

Viscosity of lube oil is determined by the Society of Automotive Engineers (SAE).

Lube oils can be multigrade or monograde where multigrade oils fulfills two viscosity specifications. Example SAE 10W-40 where 10W refers to low-temperature - or winter - viscosity and 40 refers to the high-temperature - or summer - viscosity.

Motor oil viscosity

Motor Oils - Dynamic Viscosities

SAE
Dynamic Viscosity (N s/m2)
Temperature (oC)
02050100
10 0.31 0.079 0.020 0.005
20 0.72 0.170 0.033 0.007
30 1.53 0.310 0.061 0.010
40 2.61 0.430 0.072 0.012
50 3.82 0.630 0.097 0.015
  • 1 N s/m2 = 1 kg/(m s) = 1 Pa s = 1000 cP

Dynamic viscosity chart - SAE vs. temperature

Download and print Dynamic Viscosity Chart - SAE vs. temperature