SAE MultigradeViscosityDensity
Centistokes10-6 reyns (lb s/in2)kg/m3lb/in3
40 oC100 oC104 oF 212 oF
5W-30 64 11 8.2 1 860 0.0311
10W-30 69 11 8.8 1.1 865 0.0312
10W-40 94 14.3 11.9 1.5 865 0.0312
20W-50 166 18.7 21.3 2.7 872 0.0315

 