Molybdenum Binary Eutectic Alloys - Melting Points

Mo - Molybdenum - binary eutectic alloys and melting points.

The melting point of an alloy of two (binary) or more metals depends on the relative proportions of the ingredients.

  • an eutectic mixture is the mixture where the melting point is as low as possible

Binary eutectic Molybdenum - Mo - alloys, with composition and melting points are indicated below:

Molybdenum Binary Eutectic Alloys - Melting Points
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Nb - Niobium (Columbium) 65 2570 4167
Ni - Nickel 52 1590 2403
Os - Osmium 34 2650 4311
Pd - Palladium 57 2020 3177
Re - Rhenium 64 2780 4545
Ru - Ruthenium 42 2200 3501
Si - Silicon 5.7 2350 3771
  • T (oC) = 5/9 (T (oF) - 32)