Arsenic - Melting Points of Binary Eutectic Alloys

As - Arsenic - binary eutectic alloys and their melting points.

The melting point of an alloy of two (binary) or more metals depends on the relative proportions of the ingredients.

  • an eutectic mixture is the mixture where the melting point is as low as possible

Binary eutectic Arsenic - As - alloys, with composition and melting points are indicated below:

Arsenic - Melting Points of Binary Eutectic Alloys
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Co - Cobalt 70 1189 1681
Cu - Copper 78 958 1265
Fe - Iron (Ferrum) 69 1103 2017
In - Indium 18 1004 1348
Mn - Manganese 49 1143 1598
Ni - Nickel 57 1077 1479
Sb - Antimony (Stibium) 87 878 1121
Sn - Tin (Stannum) 51 852 1074
Zn - Zinc 18 996 1333