Binary eutectic Nickel - Ni - alloys, with composition and melting points are indicated below:

Nickel Binary Eutectic Alloys - Melting Points
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Sb - Antimony (Stibium) 36.9 1375 2016
Sn - Tin (Stannum) 32.2 1403 2066
Th - Thorium 68 1303 1886
Ti - Titanium 34 1390 2043
V - Vanadium 48 1473 2192
W - Tungsten (Wolfram) 45 1773 2732
Zn - Zinc 71 1148 1607