Silver Binary Eutectic Alloys - Melting Points

Ag - Silver - binary eutectic alloys and melting points.

The melting point of an alloy of two (binary) or more metals depends on the relative proportions of the ingredients.

  • an eutectic mixture is the mixture where the melting point is as low as possible

Binary eutectic Silver - Ag - alloys, with composition and melting points are indicated below:

Silver Binary Eutectic Alloys - Melting Points
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Al - Aluminum 25 835 1044
As - Arsenic 18 813 1004
Ca - Calcium 18 820 1017
Ce - Cerium 84 798 977
Cu - Copper 28 1050 1431
Ge - Germanium 18 924 1204
La - Lanthanum 77 791 964
Li - Lithium 89 418 293
Mg - Magnesium 52 745 882
Pb - Lead (Plumbum) 97.5 577 579
Pd - Palladium 25.6 924 1204
Sb - Antimony (Stibium) 44 758 905
Si - Silicon 2.96 1110 1539
Sr - Strontium 73 709 817
Te - Tellurium 69 623 662
Th - Thorium 15 1167 1641
Zr - Zirconium 93 1100 1521
  • T (oC) = 5/9 (T (oF) - 32)