Aluminum - Melting Points of Binary Eutectic Alloys

Al - Aluminum - binary eutectic alloys and their melting points.

The melting point of an alloy of two (binary) or more metals depends on the relative proportions of the ingredients.

  • an eutectic mixture is the mixture where the melting point is as low as possible

Binary eutectic Aluminum - Al - alloys, with composition and melting points are indicated below:

Aluminum - Melting Points of Binary Eutectic Alloys
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Au - Gold (Aurum) 90 842 1056
Ca - Calcium 73 818 1013
Cd - Cadmium 90 1650 2511
Ce - Cerium 92 928 1211
Cu - Copper 33 821 1018
Fe - Iron (Ferrum) 49.34 1426 2107
Ge - Germanium 55 700 801
In - Indium 18 910 1179
Mg - Magnesium 67 710 819
Ni - Nickel 87 1658 2525
Pt - Platinum 90 1533 2300
Si - Silicon 13 850 1071
Th - Thorium 97 1510 2259
Zn - Zinc 95 655 720