Binary eutectic Iron - Fe - alloys, with composition and melting points are indicated below:

Fe - Iron - binary eutectic alloys and melting points
Alloy ComponentWeight of Alloy Component
(%)
Melting Point
KoF
Gd - Gadolinium 86 1123 1562
Mo - Molybdenum 31 1725 2646
Nb - Niobium (Columbium) 18.5 1643 2498
Sb - Antimony (Stibium) 94.1 1021 1378
Si - Silicon 21 1475 2196
Sn - Tin (Stannum) 49 1400 2061
Y - Yttrium 75 1173 1652
Zr - Zirconium 17 1600 2421