Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

ASTM B43 - Seamless Red Brass Pipes - Dimensions

Standard sizes specification for seamless red brass pipes.

Standard dimensions for seamless red brass pipe according ASTM B4:

Regular

ASTM B43 - Seamless Red Brass Pipes - Dimensions - Regular
Nominal SizeOutside DiameterWall ThicknessWeight
(in)(in)(mm)(in)(mm)(lb/ft)(kg/m)
1/8 0.405 10.3 0.062 1.57 0.253 0.376
1/4 0.540 13.7 0.082 2.08 0.447 0.665
3/8 0.675 17.1 0.090 2.29 0.627 0.993
1/2 0.840 21.3 0.107 2.72 0.934 1.39
3/4 1.050 26.7 0.114 2.90 1.27 1.89
1 1.315 33.4 0.126 3.20 1.78 2.65
1 1/4 1.660 42.2 0.146 3.71 2.63 3.91
1 1/2 1.900 48.3 0.150 3.81 3.13 4.66
2 2.375 60.3 0.156 3.96 4.12 6.13
2 1/2 2.875 73.0 0.187 4.75 5.99 8.91
3 3.500 88.9 0.219 5.56 8.56 12.7
3 1/2 4.000 102 0.250 6.35 11.2 16.7
4 4.500 114 0.250 6.35 12.7 18.9
5 5.562 141 0.250 6.35 15.8 23.5
6 6.625 168 0.250 6.35 19.0 28.3
8 8.625 219 0.312 7.92 30.9 46.0
10 10.750 273 0.365 9.27 45.2 67.3
12 12.750 324 0.375 9.52 55.3 82.3

Extra Strong

ASTM B43 - Seamless Red Brass Pipes - Dimensions - Extra Strong
Nominal SizeOutside DiameterWall ThicknessWeight
(in)(in)(mm)(in)(mm)(lb/ft)(kg/m)
1/8 0.405 10.3 0.100 2.54 0.363 0.540
1/4 0.540 13.7 0.123 3.12 0.611 0.909
3/8 0.675 17.1 0.127 3.23 0.829 1.23
1/2 0.840 21.3 0.149 3.78 1.23 1.83
3/4 1.050 26.7 0.157 3.99 1.67 2.48
1 1.315 33.4 0.182 4.62 2.46 3.66
1 1/4 1.660 42.2 0.194 4.93 3.39 5.04
1 1/2 1.900 48.3 0.203 5.16 4.10 6.10
2 2.375 60.3 0.221 5.61 5.67 8.44
2 1/2 2.875 73.0 0.280 7.11 8.66 12.9
3 3.500 88.9 0.304 7.72 11.6 17.3
3 1/2 4.000 102 0.321 8.15 14.1 21.0
4 4.500 114 0.341 8.66 16.9 25.1
5 5.562 141 0.375 9.52 23.2 34.5
6 6.625 168 0.437 11.1 32.2 47.9
8 8.625 219 0.500 12.7 48.4 72.0
10 10.750 273 0.500 12.7 61.1 90.9