Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Brass Pipes - Allowable Pressure vs. Temperature and Size

Allowable pressure for red brass 85% pipes .

Allowable pressure for red brass 85% pipe with threaded ends.

Regular Pipe

Brass Regular Pipes - Allowable Pressure vs. Temperature and Size
Nominal Size
(in)
Allowable Pressure (psi)
Temperature (oF)
100200300
1/8 370 370 320
1/4 870 870 760
3/8 890 890 780
1/2 900 900 790
3/4 810 810 710
1 630 630 560
1 1/4 690 690 610
1 1/2 630 630 560
2 540 540 480
2 1/2 450 450 390
3 510 510 450
3 1/2 570 570 500
4 510 510 440
5 410 410 360
6 340 340 300

Extra Strong Pipe (XS)

Brass Extra Strong Pipes - Allowable Pressure vs. Temperature and Size
Nominal Size
(in)
Allowable Pressure (psi)
Temperature (oF)
100200300
1/8 1960 1960 1710
1/4 2210 2210 1930
3/8 1840 1840 1610
1/2 1760 1760 1540
3/4 1510 1510 1320
1 1340 1340 1180
1 1/4 1160 1160 1020
1 1/2 1090 1090 960
2 1000 1000 870
2 1/2 970 970 850
3 910 910 790
3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!