ASTM B42 - Seamless Copper Pipes - Dimensions

Dimensions of seamless copper pipes according ASTM B42.

Seamless copper pipe according ASTM B42 Standard Specification for Seamless Copper Pipe, Standard Sizes:

Regular

ASTM B42 - Seamless Copper Pipes - Dimensions Regular
Nominal Pipe Size
(in)
Outside Diameter
(in)
Wall Thichness
(in))
Weight
(lb/ft)
1/8 0.405 0.062 0.259
1/4 0.540 0.082 0.457
3/8 0.675 0.090 0.641
1/2 0.840 0.107 0.955
3/4 1.050 0.114 1.30
1 1.315 0.126 1.82
1 1/4 1.660 0.146 2.69
1 1/2 1.900 0.150 3.20
2 2.375 0.156 4.22
2 1/2 2.875 0.187 6.12
3 3.500 0.219 8.76
3 1/2 4.000 0.250 11.4
4 4.500 0.250 12.9
5 5.562 0.250 16.2
6 6.625 0.250 19.4
8 8.625 0.312 31.6
10 10.750 0.365 46.2
12 12.750 0.375 56.5

Extra Strong

ASTM B42 - Seamless Copper Pipes - Dimensions - Strong
Nominal Pipe Size
(in)
Outside Diameter
(in))
Wall Thichness
(in))
Weight
(lb/ft)
1/8 0.405 0.100 0.371
1/4 0.540 0.123 0.625
3/8 0.675 0.127 0.847
1/2 0.840 0.149 1.25
3/4 1.050 0.157 1.71
1 1.315 0.182 2.51
1 1/4 1.660 0.194 3.46
1 1/2 1.900 0.203 4.19
2 2.375 0.221 5.80
2 1/2 2.875 0.280 8.85
3 3.500 0.304 11.8
3 1/2 4.000 0.321 14.4
4 4.500 0.341 17.3
5 5.562 0.375 23.7
6 6.625 0.437 32.9
8 8.625 0.500 49.5
10 10.750 0.500 62.4