PVDF - PolyVinylidene Fluoride Pipes - Supports

Maximum distance between PVDF pipe supports.

Maximum support spacing for PVDF - PolyVinylidene Fluoride - pipes depends on the operating temperature. Maximum spacing between supports at different temperatures can be found in the tables below:

PVDF Pipe - Schedule 40

PVDF -  PolyVinylidene Fluoride Pipes Schedule 40 - Supports
NPS
(inches)
Maximum Support Spacing (feet)
Operating Temperature (oF)
801001401)
1/2 3 1/2 3 1/2 2
3/4 4 3 1/2 2 1/2
1 4 4 2 1/2
1 1/2 4 1/2 4 1/2 2 1/2
2 4 1/2 4 1/2 2 1/2

PVDF Pipe - Schedule 80

PVDF -  PolyVinylidene Fluoride Pipes Schedule 80 - Supports
NPS
(inches)
Maximum Support Spacing (feet)
Operating Temperature (oF)
801001401)
1/2 4 1/2 4 1/2 2 1/2
3/4 4 1/2 4 1/2 3
1 5 4 1/2 3
1 1/2 5 1/2 5 3
2 5 1/2 5 3
  • 1 ft (foot) = 0.3048 m
  • T (oC) = 5/9 (T (oF) - 32)

1) For temperatures above 140 oF continuous support of the pipes is needed.

PVDF is recognized by its high mechanical strength and excellent chemical resistance even at higher temperatures.