Stainless Steel - Comparing International Standards
USAFranceGermanyGermanyItalyJapanRussiaSpainSwedenUKEuropean Union
AISIAFNORDIN 17006W.N. 17007UNIJISGOSTUNESISBSIEURONORM
201 1) SUS 201
301 1) Z 12 CN 17-07 X 12 CrNi 17 7 1.4310 X 12 CrNi 1707 SUS 301 X 12 CrNi 17-07 23 31 301S21 X 12 CrNi 17 7
302 1) Z 10 CN 18-09 X 5 CrNi 18 7 1.4319 X 10 CrNi 1809 SUS 302 12KH18N9 X 10 CrNi 18-09 23 31 302S25 X 10 CrNi 18 9
303 1) Z 10 CNF 18-09 X 10 CrNiS 18 9 1.4305 X 10 CrNiS 1809 SUS 303 X 10 CrNiS 18-09 23 46 303S21 X 10 CrNiS 18 9
303 Se 1) Z 10 CNF 18-09 X 10 CrNiS 1809 SUS 303 Se 12KH18N10E X 10 CrNiS 18-09 303S41
304 1) Z 6 CN 18-09 X 5 CrNi 18 10 X 5 CrNi 18 12 1.4301 1.4303 X 5 CrNi 1810 SUS 304 08KH18N10 06KH18N11 X 6 CrNi 19-10 23 32 304S15 304S16 X 6 CrNi 18 10
304 N 1) X 5 CrNiN 1810 SUS 304N1
304 H 1) X 8 CrNi 1910 SUS F 304H X 6 CrNi 19-10
304 L 1) Z 2 CN 18-10 X 2 CrNi 18 11 1.4306 X 2 CrNi 1911 SUS 304L 03KH18N11 X 2 CrNi 19-10 23 52 304S11 X 3 CrNi 18 10
Z 2 CN 18-10-Az X 2 CrNiN 18 10 1.4311 X 2 CrNiN 1811 SUS 304LN 23 71
305 1) Z 8 CN 18-12 X 8 CrNi 1812 SUS 305 X 8 CrNi 18-12 23 33 305S19 X 8 CrNi 18 12
Z 6 CNU 18-10 SUS XM7 X 6 CrNiCu 18 10 4 Kd
309 1) Z 15 CN 24-13 X 15 CrNiS 20 12 1.4828 X 16 CrNi 2314 SUH 309 309S24 X 15 CrNi 23 13
309 S 1) X 6 CrNi 2314 SUS 309S 20KH23N18 X 6 CrNi 22 13
310 1) X 12 CrNi 25 21 1.4845 X 22 CrNi 2520 SUH 310 10KH23N18 310S24
310 S 1) Z 12 CN 25-20 X 12 CrNi 25 20 1.4842 X 5 CrNi 2520 SUS 310S 20KH25N20S2 23 61 X 6 CrNi 25 20
314 1) Z 12 CNS 25-20 X 15 CrNiSi 25 20 1.4841 X 16 CrNiSi 2520 X 15 CrNiSi 25 20
316 1) Z 6 CND 17-11 X 5 CrNiMo 17 12 2 1.4401 X 5 CrNiMo 1712 SUS 316 X 6 CrNiMo 17-12-03 23 47 316S31 X 6 CrNiMo 17 12 2
316 1) Z 6 CND 17-12 X 5 CrNiMo 17 13 3 1.4436 X 5 CrNiMo 1713 SUS 316 X 6 CrNiMo 17-12-03 23 43 316S33 X 6 CrNiMo 17 13 3
316 F 1) X 12 CrNiMoS 18 11 1.4427
316 N 1) SUS 316N
316 H 1) X 8 CrNiMo 1712 SUS F 316H X 5 CrNiMo 17-12
316 H 1) X 8 CrNiMo 1713 03KH17N14M2 X 6 CrNiMo 17-12-03
316 L 1) Z 2 CND 17-12 X 2 CrNiMo 17 13 2 1.4404 X 2 CrNiMo 1712 SUS 316L X 2 CrNiMo 17-12-03 23 48 316S11 X 3 CrNiMo 17 12 2
Z 2 CND 17-12-Az X 2 CrNiMoN 17 12 2 1.4406 X 2 CrNiMoN 1712 SUS 316LN 03KH16N15M3
316 L 1) Z 2 CND 17-13 X 2 CrNiMo 18 14 3 1.4435 X 2 CrNiMo 1713 X 2 CrNiMo 17-12-03 23 53 316S13 X 3 CrNiMo 17 13 3
Z 2 CND 17-13-Az X 2 CrNiMoN 17 13 3 1.4429 X 2 CrNiMoN 1713 08KH17N13M2T 10KH17N13M2T 23 75
Z6 CNDT 17-12 X 6 CrNiMoTi 17 12 2 1.4571 X 6 CrNiMoTi 1712 08KH17N13M2T 10KH17N13M2T X 6 CrNiMoTi 17-12-03 23 50 320S31 X 6 CrNiMoTi 17 12 2
X 10 CrNiMoTi 18 12 1.4573 X 6 CrNiMoTi 1713 08KH16N13M2B X 6 CrNiMoTi 17-12-03 320S33 X 6 CrNiMoTI 17 13 3
Z 6 CNDNb 17-12 X 6 CrNiMoNb 17 12 2 1.4580 X 6 CrNiMoNb 1712 09KH16N15M3B X 6 CrNiMoNb 17 12 2
X 10 CrNiMoNb 18 12 1.4583 X 6 CrNiMoNb 1713 X 6 CrNiMoNb 17 13 3
317 1) X 5 CrNiMo 1815 SUS 317 23 66 317S16
317 L 1) Z 2 CND 19-15 X 2 CrNiMo 18 16 4 1.4438 X 2 CrNiMo 1815 SUS 317L 23 67 317S12 X 3 CrNiMo 18 16 4
317 L 1) Z 2 CND 19-15 X 2 CrNiMo 18 16 4 1.4438 X 2 CrNiMo 1816 SUS 317L 23 67 317S12 X 3 CrNiMo 18 16 4
330 1) Z 12NCS 35-16 X 12 NiCrSi 36 16 1.4864 SUH 330 08KH18N10T
321 1) Z 6 CNT 18-10 X 6 CrNiTi 18 10 X 12 CrNiTi 18 9 1.4541 1.4878 X 6 CrNiTi 1811 SUS 321 12KH18N10T X 6 CrNiTi 18-11 23 37 321S31 X 6 CrNiTi 18 10
321 H 1) X 8 CrNiTi 1811 SUS 321H X 7 CrNiTi 18-11 321S20
329 1) X 8 CrNiMo 27 5 1.4460 SUS 329J1 08KH18N12B 23 24
347 1) Z 6 CNNb 18-10 X 6 CrNiNb 18 10 1.4550 X 6 CrNiNb 1811 SUS 347 X 6 CrNiNb 18-11 23 38 347S31 X 6 CrNiNb 18 10
347 H 1) X 8 CrNiNb 1811 SUS F 347H X 7 CrNiNb 18-11
904L 1) Z 12 CNDV 12-02 1.4939
X 20 CrNiSi 25 4 1.4821
UNS31803 2) X 2 CrNiMoN 22 5 1.4462
UNS32760 2) Z 3 CND 25-06Az X 3 CrNiMoN 25 7 1.4501 12Kh13
403 3) Z 12 C 13 X 6 Cr 13 X 10 Cr 13 X 15 Cr 13 1.4000 1.4006 1.4024 X 12 Cr 13 SUS 403 X 6 Cr 13 23 02 403S17 X 10 Cr 13 X 12 Cr 13
405 3) Z 6 CA 13 X 6 CrAl 13 1.4002 X 6 CrAl 13 SUS 405 X 6 CrAl 13 405S17 X 6 CrAl 13
Z 8 CA 7 X 10 CrAl 7 1.4713 10Kh13SYu X 10 CrAl 7
X 10 CrAl 13 1.4724 X 10 CrAl 12 15Kh18SYu
X 10 CrAl 18 1.4742 X 10 CrSiAl 18
409 3) Z 6 CT 12 X 6 CrTi 12 1.4512 X 6 CrTi 12 SUH 409 409S19 X 5 CrTi 12
X 2 CrTi 12 12Kh13
410 3) Z 10 C 13 Z 12 C 13 X 6 Cr 13 X 10 Cr 13 X 15 Cr 13 1.4000 1.4006 1.4024 X 12 Cr 13 SUS 410 08Kh13 X 12 Cr 13 23 02 410S21 X 12 Cr 13
410 S 3) Z 6 C 13 X 6 Cr 13 1.4000 X 6 Cr 13 SUS 410S 23 01 403S17 X 6 Cr 13
414 3)

1) Austenitic grades

2) Ferritic austenitic grades, Duplex and Super Duplex

3) Ferritic grades

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter


















































9.4.10

.
Cookie Settings