Maximum distance between epoxy fiberglass pipe supports at different operating temperatures are indicated in the table below. Maximum operating temperature for epoxy pipes should not exceed 300 oF (149 oC).

Epoxy Pipes - Support Spacing
Nominal Pipe SizeTemperature
oCoFoCoFoCoFoCoFoCoFoCoF
2475661507917593200107225121250
Maximum Support Spacing
inchesmmmftmftmftmftmftmft
1 25 3.2 9.9 3.0 9.8 3.0 9.7 2.9 9.4 2.8 9.3 2.7 8.7
1 1/2 40 3.5 11.6 3.5 11.4 3.4 11.3 3.4 11.0 3.3 10.8 3.1 10.1
2 50 4.0 13.1 3.9 12.9 3.9 12.8 3.8 12.4 3.7 12.2 3.5 11.4
3 80 4.6 15.0 4.5 14.8 4.5 14.6 4.3 14.2 4.3 14.0 4.0 13.0
4 100 5.1 16.7 5.0 16.5 5.0 16.3 4.8 15.8 4.8 15.6 4.4 14.5
6 150 5.8 18.9 5.7 18.6 5.6 18.4 5.5 17.9 5.4 17.6 5 16.4
8 200 6.1 20.0 6.1 20.0 6.0 19.8 5.9 19.3 5.8 19.0 5.4 17.7
10 250 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0 5.7 18.8
12 300 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0 6.0 19.7
14 350 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0 6.1 20.0