Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

CPVC Pipes - Hanger Spacing

Maximum distance between CPVC pipe supports.

Maximum support spacing for CPVC - Chlorinated Poly Vinyl Chloride - pipes depends on the operating temperature. Maximum spacing between supports at different temperatures can be found in the tables below:

CPVC Pipes - Schedule 40

CPVC Pipes Schedule 40 - Maximum Support Spacing
NPS
(inches)
Spacing (feet)
Operating Temperature (oF)
60100140
1/2 5 4.5 4
3/4 5.5 5 4
1 6 5.5 4.5
1 1/4 6 5.5 5
1 1/2 6.5 6 5
2 6.5 6 5
3 8 7 6
4 8.5 7.5 6.5
6 9.5 8.5 7.5

CPVC Pipes - Schedule 80

CPVC Pipes Schedule 80 - Maximum Support Spacing
NPS
(inches)
Spacing (feet)
Operating Temperature (oF)
60100140
1/2 5.5 5 4.5
3/4 6 5.5 4.5
1 6.5 6 5
1 1/2 7 6.5 5.5
2 7.5 7 6
3 9 8 7
4 10 9 7.5
6 11 10 9
  • 1 ft (foot) = 0.3048 m
  • T (oC) = 5/9 (T (oF) - 32)

Chlorinated Poly Vinyl Chloride - CPVC - is a thermoplastic pipe and fitting material made with CPVC compounds meeting the requirements of ASTM Class 23447 as defined in ASTM Specification D1784.

CPVC applications are for potable water distribution, corrosive fluid handling in industry, and fire suppression systems.