Specific heat of some common polymers at 0 oC:

Polymers - Specific Heats
PolymerSpecific Heat
(J/(kg oC))
Epoxy resin, cured 1110
Nylon 6 1310
PET 1030
PMMA, Perspex 1270
Polycarbonate 1100
Polyethylene 1550
Polystyrene 1110
Rubber, natural - vulcanised or unvulvanised 1800
Polytetrafluoroethylene (PTFE) 970
PVC 880