MaterialEmissivity Coefficient
- ε -
Water (0 - 100 oC) 0.95 - 0.963
Ice 0.96 - 0.99
Snow 0.96 - 0.98
Sand 0.9
Granite 0.96
Green Grass 0.975 - 0.986