Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

PE - Polyethylene High Density Pipes - Weights

Weight of polyethylene pipes - metric units.

Approximately weights of polyethylene high density - PEH - pipes:

PE - Polyethylene High Density Pipes - Weights
Outside Diameter
(mm)
Pressure Rating
PN 2.5PN 4PN 6PN 10PN 16
Pipe Weight (kg/m)
20       0.11 0.16
25     0.13 0.17 0.24
32     0.19 0.28 0.39
40   0.21 0.29 0.44 0.61
50   0.32 0.45 0.68 0.95
63 0.33 0.48 0.70 1.1 1.5
75 0.46 0.69 0.9 1.5 2.1
90 0.65 0.99 1.4 2.2 3.1
110 0.96 1.5 2.1 3.2 4.6
125 1.3 1.9 2.7 4.1 5.9
140 1.6 2.4 3.4 5.2 7.8
160 2.0 3.1 4.4 6.8 9.6
180 2.5 3.9 5.6 8.6 12.1
200 3.1 4.8 6.9 10.6 15.0
225 3.9 6.0 8.7 13.4 19.0
250 4.9 7.4 10.7 16.4 23.4
280 6.1 9.2 13.4 20.6 29
315 7.6 11.8 17.0 26.0 37
355 9.7 14.9 21.6 33.0 47
400 12.3 18.8 27.3 41.9 60
450 15.9 24.3 35.3 54.3 77
500 19.7 30.0 43.0 67  
560 24.5 37.7 54.5 84  
600 26.9 43.7 63 96  
630 31.0 47.7 69 106  
710 39.5 60.5 88    
800 50 77 111    
900 63 97 141    
1000 78 120 173    
1200 112 172      
1400          
1600 199 306      

PE pipes are produced in different pressure grades - PN grades - indicating the pressure in bars the pipe can support with water at 20 oC.

pe pipes - pn grades and weight

The pressure grades available according to European standards are

  • PN 2.5 - max pressure 2.5 bar
  • PN 4 - max pressure 4 bar
  • PN 6 - max pressure 6 bar
  • PN 10 - max pressure 10 bar
  • PN 16 - max pressure 16 bar
  • 1 bar = 105 Pa (N/m2) = 0.1 N/mm2 = 10.197 kp/m2 = 10.20 m H2O = 0.9869 atm = 14.50 psi (lbf/in2) = 106 dyn/cm2 = 750 mmHg