Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Freezing Mixtures and Cooling Agents

Freezing mixtures, cooling agents and freezing points.

Freezing points for water with freezing mixtures based on salt and ice:

Freezing Mixtures - Temperature Ranges
Freezing MixtureTemperature Change (oF)Temperature Change (oC)
FromToFromTo
  • Ammonium Nitrate (NH4NO3) - 1 part
  • Water - 1 part
50 3 10 -16
  • Calcium Chloride (CaCl2) - 3 parts
  • Snow or ice - 2 parts
32 -27 0 -33
  • Potassium Hydrate (KOH) - 4 parts
  • Snow or ice - 3 parts
32 -35 0 -37
  • Sal Ammoniac (NH4Cl) - 5 parts
  • Saltpeter (KNO3) - 5 parts
  • Water - 16 parts
50 10 10 -12
  • Sal Ammoniac (NH4Cl) - 1 part
  • Saltpeter (KNO3) - 1 part
  • Water - 1 part
46 -11 8 -24
  • Salt (NaCl) - 1 part
  • Snow or ice - 3 parts
32 0 0 -18
  • Salt (NaCl) - 1 part
  • Snow or ice - 1part
32 -0.4 0 -18

Ammonium Nitrate - Chrushed Ice or Snow in Water

  • 1 part Ammonium Nitrate - 0.94 parts Ice/water : temperature -4 oC
  • 1 part Ammonium Nitrate - 1.20 parts Ice/water : temperature -14 oC
  • 1 part Ammonium Nitrate - 1.31 parts Ice/water : temperature -17.5 oC
  • 1 part Ammonium Nitrate - 3.61 parts Ice/water : temperature -8 oC

Calcium Chloride - Chrushed Ice or Snow in Water

  • 1 part Calcium Chloride - 0.49 parts Ice/water : temperature -20 oC
  • 1 part Calcium Chloride - 0.61 parts Ice/water : temperature -39 oC
  • 1 part Calcium Chloride - 0.70 parts Ice/water : temperature -55 oC
  • 1 part Calcium Chloride - 1.23 parts Ice/water : temperature -22 oC
  • 1 part Calcium Chloride - 4.92 parts Ice/water : temperature -4 oC

Sodium Chloride - Chrushed Ice or Snow in Water

  • 1 part Sodium Chloride - 2 parts Ice/water : temperature -18 oC

Evaporating Liquid Gases at Atmospheric Pressure

  • Liquid Oxygen : temperature -183 oC
  • Liquid Nitrogen : temperature -196 oC
  • Liquid Helium : temperature -269 oC