Cast Iron Threaded Pipe Fittings - Working Pressures vs. Temperature

Maximum working pressures for cast iron threaded pipe fittings according ANSI B16.4.

Maximum working pressures of cast iron pipe fittings - threaded fittings according ANSI B16.4:

Cast Iron Threaded Pipe Fittings - Working Pressures vs. Temperature
Temperature
(oF)

Maximum Working Pressure (psig)
Pressure Class
125250
-20 to 150 175 400
200 165 370
250 150 340
300 140 310
350 125 280
400 - 250