Welding or Melting ProcessTemperature (°C)
Oxygen hydrogen torch 1450
Combustion furnace 1700
Aluminium-iron powder 2800
Electric furnace 3000
Oxygen acetylene torch 3500
Direct electric arc 4000
Electron-beam welding > 10000
Laser-beam welding > 10000
Plasma arc welding 33000