Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Sugar Water Solutions - Viscosities

Dynamic viscosities of sucrose water solutions vs. temperature.

Sugar Water Solutions - Viscosities
Temperature
(oC)
Absolute Viscosity (cP)
Sucrose (% per weight)
204060
0 3.82 14.8
10 2.66 9.83 113
20 1.97 6.22 56.7
30 1.51 4.40 34.0
40 1.20 3.26 21.3
50 0.97 2.51 14.1
60 0.81 1.99 9.87
70 0.69 1.61 7.18
80 0.59 1.34 5.42
90 1.13 4.17
95 1.04 3.73