PE - Polyethylene High Density Water Supply Pipes - Properties

Nominal pipe size, outside diameter, wall thickness, weight and working pressure.

PE - Polyethylene High Density Water Supply Pipes - Properties
Nominal Pipe Size
(in)
Outside Diameter
(in)
Wall Thickness
(in)
Inside Diameter
(in)
Working Pressure
(psi at 73 oF)
Weight
(lb/ft)
1/2 0.800 0.089 0.622 100 0.08
0.762 0.070 0.622 75 0.06
3/4 1.060 0.118 0.824 100 0.15
0.994 0.085 0.824 75 0.10
1 1.359 0.155 1.049 100 0.23
1.265 0.108 1.049 75 0.17
1 1/4 1.772 0.196 1.380 100 0.40
1.666 0.143 1.380 75 0.28
1 1/2 2.070 0.1230 1.610 100 0.55
1.942 0.166 1.610 75 0.39
2 2.657 0.295 2.067 100 0.90
2.495 0.214 2.067 75 0.64
  • PE - Polyethylene