Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Sulfuric Acid - Density

Density of sulfuric acid at various temperatures and concentrations.

Sulfuric Acid Density - Concentration and Temperature

Sulfuric Acid - Density
Concentration
(% mass H2SO4)
Density (g/mL)
Temperature (oC)
020406080100
1 1.0074 1.0051 0.9986 0.9895 0.9779 0.9646
20 1.1510 1.1394 1.1275 1.1153 1.1021 1.0885
40 1.3179 1.3028 1.2880 1.2732 1.2589 1.2446
60 1.5154 1.4983 1.4816 1.4656 1.4497 1.4344
80 1.7482 1.7272 1.7069 1.6873 1.6680 1.6493
100 1.8517 1.8305 1.8107 1.7922
3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!