fractional Inchesdecimal Inces
Eights
1/8 0.125
1/4 0.250
3/8 0.375
1/2 0.500
5/8 0.625
3/4 0.750
7/8 0.875
Sixteenths
1/16 0.0625
3/16 0.1875
5/16 0.3125
7/16 0.4375
9/16 0.5625
11/16 0.6875
13/16 0.8125
15/16 0.9375
Thirty-seconds
1/32 0.03125
3/32 0.09375
5/32 0.15625
7/32 0.21875
9/32 0.28125
11/32 0.34375
13/32 0.40625
15/32 0.46875
17/32 0.53125
19/32 0.59375
21/32 0.65625
23/32 0.71875
25/32 0.78125
27/32 0.84375
29/32 0.90625
31/32 0.96875
Sixty-fourths
1/64 0.015625
3/64 0.046875
5/64 0.078125
7/64 0.109375
9/64 0.140625
11/64 0.171875
13/64 0.203125
15/64 0.234375
17/64 0.265625
19/64 0.296875
21/64 0.328125
23/64 0.359375
25/64 0.390625
27/64 0.421875
29/64 0.453125
31/64 0.484375
33/64 0.515625
35/64 0.546875
37/64 0.578125
39/64 0.609375
41/64 0.640625
43/64 0.671875
45/64 0.703125
47/64 0.734375
49/64 0.765625
51/64 0.796875
53/64 0.828125
55/64 0.859375
57/64 0.890625
59/64 0.921875
61/64 0.953125
63/64 0.984375

Length Units Converter

Inches - fractional to decimal converting table

Download Inches - Fraction to Decimal Converting Table

Fraction to Decimal - Example

Convert 1/8" to decimal:

  1. numerator is top number - numerator is 1
  2. denominator is bottom number - denominator is 8
  3. divide the top number with the bottom number - 1/8 = 0.125