Ice - Properties

Properties like Youngs modulus, tensile strength, compressive strength and fracture of toughness for ice.

  • Youngs modulus of elasticity E (GPa): 9.1
  • Fracture of toughness Kc (MPa m1/2): 0.12
  • Ultimate tensile strength σu (MPa): 1
  • Compressive strength σc (MPa): 6