Some of the fiberglass related standards from the major standardization organizations:

ASME Standards

Fiberglass related standards from ASME - American Society of Mechanical Engineers:

ASTM Standards

Fiberglass related standards from ASTM International

  • ASTM C 581 - STANDARD PRACTICE FOR DETERMINING CHEMICAL RESISTANCE OF THERMOSETTING RESINS USED IN GLASS-FIBER-REINFORCED STRUCTURES INTENDED FOR LIQUID SERVICE
  • ASTM C 582 - STANDARD SPECIFICATION FOR CONTACT-MOLDED REINFORCED THERMOSETTING PLASTIC (RTP) LAMINATES FOR CORROSION RESISTANT EQUIPMENT
  • ASTM D 149 - STANDARD TEST METHOD FOR DIELECTRIC BREAKDOWN VOLTAGE AND DIELECTRIC STRENGTH OF SOLID ELECTRICAL INSULATING MATERIALS AT COMMERCIAL POWER FREQUENCIES
  • ASTM D 257 - TEST METHODS FOR DC RESISTANCE OR CONDUCTANCE OF INSULATING MATERIALS
  • ASTM D 638 - STANDARD TEST METHOD FOR TENSILE PROPERTIES OF PLASTICS
  • ASTM D 695M - TEST METHOD FOR COMPRESSIVE PROPERTIES OF RIGID PLASTICS (METRIC)
  • ASTM D 696 - STANDARD TEST METHOD FOR COEFFICIENT OF LINEAR THERMAL EXPANSION OF PLASTICS BETWEEN - 30 DEGREES C AND 30 DEGREES C WITH A VITREOUS SILICA DILATOMETER
  • ASTM D 790 - STANDARD TEST METHODS FOR FLEXURAL PROPERTIES OF UNREINFORCED AND REINFORCED PLASTICS AND ELECTRICAL INSULATING MATERIALS
  • ASTM D 792 - TEST METHODS FOR DENSITY AND SPECIFIC GRAVITY (RELATIVE DENSITY) OF PLASTICS BY DISPLACEMENT
  • ASTM D 1598 - STANDARD TEST METHOD FOR TIME-TO-FAILURE OF PLASTIC PIPE UNDER CONSTANT INTERNAL PRESSURE
  • ASTM D 1599 - STANDARD TEST METHOD FOR RESISTANCE TO SHORT-TIME HYDRAULIC PRESSURE OF PLASTIC PIPE, TUBING, AND FITTINGS
  • ASTM D 2105 - STANDARD TEST METHOD FOR LONGITUDINAL TENSILE PROPERTIES OF "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE AND TUBE
  • ASTM D 2143 - STANDARD TEST METHOD FOR CYCLIC PRESSURE STRENGTH OF REINFORCED, THERMOSETTING PLASTIC PIPE
  • ASTM D 2290 - STANDARD TEST METHOD FOR APPARENT HOOP TENSILE STRENGTH OF PLASTICOR REINFORCED PLASTIC PIPE BY SPLIT DISK METHOD
  • ASTM D 2310 - STANDARD CLASSIFICATION FOR MACHINE-MADE "FIBERGLASS" (GLASS-FIBER REINFORCED THERMOSETTING-RESIN) PIPE
  • ASTM D 2412 - STANDARD TEST METHOD FOR DETERMINATION OF EXTERNAL LOADING CHARACTERISTICS OF PLASTIC PIPE BY PARALLEL-PLATE LOADING
  • ASTM D 2444 - TEST METHOD FOR DETERMINATION OF THE IMPACT RESISTANCE OF THERMOPLASTIC PIPE AND FITTINGS BY MEANS OF A TUP (FALLING WEIGHT)
  • ASTM D 2583 - STANDARD TEST METHOD FOR INDENTATION HARDNESS OF RIGID PLASTICS BY MEANS OF A BARCOL IMPRESSOR
  • ASTM D 2584 - STANDARD TEST METHOD FOR IGNITION LOSS OF CURED REINFORCED RESINS
  • ASTM D 2924 - STANDARD TEST METHOD FOR EXTERNAL PRESSURE RESISTANCE OF "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE
  • ASTM D 2925 - STANDARD TEST METHOD FOR BEAM DEFLECTION OF "FIBERGLASS" (GLASS- FIBER-REINFORCED THERMOSETTING RESIN) PIPE UNDER FULL BORE FLOW
  • ASTM D 2992 - STANDARD PRACTICE FOR OBTAINING HYDROSTATIC OR PRESSURE DESIGN BASIS FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE AND FITTINGS
  • ASTM D 2996 - STANDARD SPECIFICATION FOR FILAMENT-WOUND "FIBERGLASS" (GLASS- FIBER-REINFORCED THERMOSETTING-RESIN) PIPE
  • ASTM D 2997 - STANDARD SPECIFICATION FOR CENTRIFUGALLY CAST "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE
  • ASTM D 3262 - STANDARD SPECIFICATION FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) SEWER PIPE
  • ASTM D 3517 - STANDARD SPECIFICATION FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PRESSURE PIPE
  • ASTM D 3567 - STANDARD PRACTICE FOR DETERMINING DIMENSIONS "FIBERGLASS" (GLASS- FIBER-REINFORCED THERMOSETTING RESIN) PIPE AND FITTINGS
  • ASTM D 3615 - CHEMICAL RESISTANCE OF THERMOSET MOLDING COMPOUNDS
  • ASTM D 3681 - STANDARD TEST METHOD FOR CHEMICAL RESISTANCE OF "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE IN A DEFLECTED CONDITION
  • ASTM D 3754 - STANDARD SPECIFICATION FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) SEWER AND INDUSTRIAL PRESSURE PIPE
  • ASTM D 3840 - STANDARD SPECIFICATION FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE FITTINGS FOR NONPRESSURE APPLICATIONS
  • ASTM D 4024 - STANDARD SPECIFICATION FOR MACHINE MADE "FIBERGLASS" (GLASS-FIBER REINFORCED THERMOSETTING RESIN) FLANGES
  • ASTM D 4161 - STANDARD SPECIFICATION FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE JOINTS USING FLEXIBLE ELASTOMERIC SEALS
  • ASTM D 5365 - STANDARD TEST METHOD FOR LONG-TERM RING-BENDING STRAIN OF "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE
  • ASTM D 5421 - STANDARD SPECIFICATION FOR CONTACT MOLDED "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING RESIN) FLANGES
  • ASTM D 5677 - STANDARD SPECIFICATION FOR FIBERGLASS (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PIPE AND PIPE FITTINGS, ADHESIVE BONDED JOINT TYPE, FOR AVIATION JET TURBINE FUEL LINES
  • ASTM D 5685 - STANDARD SPECIFICATION FOR "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING-RESIN) PRESSURE PIPE FITTINGS
  • ASTM D 6041 - STANDARD SPECIFICATION FOR CONTACT-MOLDED "FIBERGLASS" (GLASS-FIBER-REINFORCED THERMOSETTING RESIN) CORROSION RESISTANT PIPE AND FITTINGS
  • ASTM E 228 - LINEAR THERMAL EXPANSION OF SOLID MATERIALS WITH A VITREOUS SILICA DILATOMETER
  • ASTM F 1173 - STANDARD SPECIFICATION FOR THERMOSETTING RESIN FIBERGLASS PIPE SYSTEMS TO BE USED FOR MARINE APPLICATIONS

AWWA Standards

Fiberglass related standards from AWWA - American Water Works Association

  • AWWA C950-01 - Fiberglass Pressure Pipe
  • AWWA D120-84 (R89) - Thermosetting Fiberglass-Reinforced Plastic Tanks
  • AWWA F101-02 - Contact-Molded, Fiberglass-Reinforced Plastic Wash Water Troughs and Launders
  • AWWA F102-02 - Matched-Die-Molded, Fiberglass-Reinforced Plastic Weir Plates, Scum Baffles, and Mounting Brackets

BSi Standards

Fiberglass related standards from BSi - British Standards institute

  • BS 5480 - Specification for glass reinforced plastics (GRP) pipes, joints and fittings for use for water supply or sewerage
  • BS 6464 - Specification for reinforced plastics pipes, fittings and joints for process plants
  • BS 7159 - Code of practice for design and construction of glass-reinforced plastics (GRP) piping systems for individual plants or sites
  • BS 8010-2.5 - Code of practice for pipelines - Pipelines on land: design, construction and installation - Glass reinforced thermosetting plastics

DIN Standards

Fiberglass related standards from DIN - Deutsches Institut für Normung

  • DIN 53393 - Testing of Textile Glass-reinforced Plastics; Behavior to the Effect of Chemicals
  • DIN 53758 - Testing of plastics articles; determination of the effect of internal pressure on hollow objects by short-time test
  • DIN 53768 - Determination by extrapolation of the long-term behavior of glass fiber reinforced plastics
  • DIN 53769-1 - Testing of glass fiber reinforced plastics pipes; determination of the longitudinal shear strength of type B pipe fittings
  • DIN 53769-2 - Testing of glass fiber reinforced plastics pipes; long-term hydrostatic pressure test
  • DIN 53769-3 - Testing of glass fiber reinforced plastics pipes; determination of initial and long-term ring stiffness
  • DIN 53769-6 - Testing of glass fiber reinforced plastics pipes; Testing of pipes and fittings under pulsating internal pressure
  • DIN EN 59 - Glass Reinforced Plastics; Measurement of Hardness by Means of a Barcol Impressor
  • DIN EN 637 - Plastics piping systems - Glass-reinforced plastics components - Determination of the amounts of constituents using the gravimetric method
  • DIN EN 705 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes and fittings - Methods for regression analyses and their use
  • DIN EN 761 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of the creep factor under dry conditions
  • DIN EN 1393 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes; Determination of initial longitudinal tensile properties
  • DIN EN 1447 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of long-term resistance to internal pressure
  • DIN EN 1448 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) components - Test methods to prove the design of rigid locked socket- and -spigot joints with elastomeric seals
  • DIN EN 1449 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) components - Test methods to prove the design of a cemented socket- and -spigot joints
  • DIN EN 1450 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) components - Test methods to prove the design of bolted flange joints

ISO Standards

Fiberglass related standards from ISO - International Organization for Standardization

  • ISO 178 - Plastics - Determination of flexural properties
  • ISO 527-4 - Plastics - Determination of tensile properties - Part 4: Test conditions for isotropic and orthotropic fibre-reinforced plastic composites
  • ISO 7370 - Glass fiber reinforced thermosetting plastics (GRP) pipes and fittings; Nominal diameters, specified diameters and standard lengths
  • ISO 7510 - Plastics piping systems - Glass-reinforced plastics (GRP) components - Determination of the amounts of constituents using the gravimetric method
  • ISO 7684 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of the creep factor under dry conditions
  • ISO 10466 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Test method to prove the resistance to initial ring deflection
  • ISO 10928 - Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes and fittings - Methods for regression analysis and their use
  • ISO/TR 10465-1 - Underground installation of flexible glass-reinforced thermosetting resin (GRP) pipes; part 1: installation procedures
  • ISO/TR 10465-2 - Underground installation of flexible glass-reinforced thermosetting resin (GRP) pipes - Part 2: Comparison of static calculation methods
  • ISO/TR 10465-3 - Underground installation of flexible glass-reinforced thermosetting resin (GRP) pipes - Part 3: Installation parameters and application limits
3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter


















































9.19.10

.
Cookie Settings