MaterialsForgingsCastingsWrought FittingsPipe
Carbon Steel A181-Gr.1 A181-Gr.2 A234-WPA WPB WPC
Moderate, high temp. service A105-Gr.1 A105-Gr.2 A216-WCA WCB WCC A106-Gr.B/API 5 LB
Cold temp. service A350-LF1 A350-LF2 A352-LCB, LCC A420-WPL6 A33-Gr.6/A 671
Carbon -1/2 Moly Alloy Steel
High Temp Service A182-F1 A217-WC1 A234-WP1
Cold Temp Service A352-LC1
1/2Cr-1/2Mo Alloy Steel A182-F2
1/2Cr-1/2Mo-1 Alloy Steel A217-WC4
3/4Cr-1 Mo-3/4NI Alloy Steel A217-WC5
1Cr-1/2Mo Alloy Steel A182-F12 A234-WP12
1Cr-1 Mo-Vd Alloy Steel A404-F24 A389-C24
1-1/4Cr-1/2Mo Alloy Steel A182-F11 A217-WC6 A234-WP11
1-1/4Cr-1/2Mo-Vd Alloy Steel A389-C23
2-1/4Cr-1/2Mo-Vd Alloy Steel A182-F22 A217-WC9 A234-WP22
3Cr-1 Mo Alloy Steel A182-F21
5Cr-1/2Mo Alloy Steel A182-F5 A234-WP5
5Cr-1/2Mo-Si Alloy Steel A217-Gr.C5
7Cr-1/2Mo Alloy Steel A182-F7 A234-WP7
9Cr-1 Mo Alloy Steel A182-F9 A217-Gr.C12 A234-WP9
13Cr Alloy Steel A182-F6 A351-CA15
Type 304 Stainless Steel
Standard A182-F304 A351-Gr.CF8 CF8a A403-WP304 A312-TP304
Low Carbon A182-F304-L A351-Gr.CF3 CF3a A403-WP304-L A312-Tp304L
High Temp Service A182-F304-H A351.Gr.CF10 A403-WP304-H A312-TP304H
Type 309 Stainless Steel A403-WP309
Type 310 Stainless Steel A182-F310 A403-WP310 A312-TP310
Type 316 Stainless Steel
Standard A182-F316 A351-Gr.CF8M A403-WP316 A312-TP316
Low Carbon A182-F316-L A351-Gr.CF3M A403-WP316-L A312-TP316L
High Temp Service A182-F316-H A351.Gr.CF10 A403-WP316-H A312-TP316H
Type 317 Stainless Steel A403-WP317
Type 321 Stainless Steel
Standard A182-F321 A403-WP321
High Temp Service A182-F321-H A403-WP321-H
Type 347 Stainless Steel
Standard A182-F347 A403-WP347
High Temp Service A182-F347-H A351-Gr.CF8C A403-WP347-H
Type 348 Stainless Steel
Standard A182-F348 A403-WP348
High Temp Service A182-F348-H
20 Ni-8 Cr Alloy A182-F10