ANSI B16.5 - Steel Pipe Flanges - Pressure and Temperature Ratings - Group 1.2.

Pressure (psig) and temperature ratings for steel pipe flanges and flanged fittings

Pressure (psig) and temperature ratings for steel pipe flanges and flanged fittings according the American National Standard ANSI B16.5 - 1988 Group 1.2:

For full table - rotate the screen!

ANSI B16.5 - Steel Pipe Flanges - Pressure and Temperature Ratings - Group 1.2.
Temperature (°C)
Working Pressure (bar)
Class
15030040060090015002500
-29 - 38 19.8 51.7 68.9 103.4 155 259 431
50 19.5 51.7 68.9 103.4 155 259 431
100 17.7 51.5 68.7 103.0 155 258 429
150 15.8 50.2 66.8 100.3 151 251 418
200 13.8 48.6 64.8 97.2 146 243 405
250 12.1 46.3 61.7 92.7 139 232 386
300 10.2 42.9 57.0 85.7 129 214 357
325 9.3 41.4 55.0 82.6 124 207 344
350 8.4 40.0 53.4 80.0 120 200 334
375 7.4 37.8 50.4 75.7 114 189 315
400 6.5 34.7 46.3 69.4 104 174 290
425 5.5 28.8 38.4 57.5 86.3 144 240
450 4.6 23.0 30.7 46.0 69.0 115 192
475 3.7 17.1 22.8 34.2 51.3 85.4 142
500 2.8 11.6 15.4 23.2 34.7 57.9 96.5
538 1.4 5.9 7.9 11.8 17.7 29.5 49.2

The values in this table apply to materials Group 1.2

For other Material Groups the Pressure-Temperature Ratings are different. Most carbon steels are only acceptable for temperatures below 800 F.