Dimensions of PVC pipes according ASTM D2665 Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Drain, Waste, and Vent Pipe and Fittings.

ASTM D2665 - Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Drain, Waste, and Vent Pipe and Fittings - Dimensions
Nominal Pipe Size
(in)
Average Outside Diameter
(in)
Wall Thickness
(in)
Weight
(lb/ft)
1 1/4 1.660 0.140 0.65
1 1/2 1.900 0.145 0.78
2 2.375 0.154 1.1
3 3.500 0.216 2.2
4 4.500 0.237 3.1
6 6.625 0.280 5.4
8 8.625 0.322 8.2
10 10.750 0.365 11.6
12 12.750 0.406 15.3
14 14.000 0.437 18.1
16 16.000 0.500 23.7
18 18.000 0.562 30.1
20 20.000 0.593 36.1
24 24.000 0.687 50.2

For sizes 1 1/4" and larger ASTM D2665 for DWV pipe is comparable to ASTM D1785 Schedule 40.